常用塑料加工温度参考表
|
塑料名称 |
千燥时间h |
注射温度℃ |
|
PC |
4-6 |
270-310 |
|
TPU |
2-4 |
190-220 |
|
LCP |
2-4 |
350-380 |
|
PPS |
3-5 |
320-340 |
|
PBT |
4-6 |
220-270 |
|
PET |
4-6 |
260-310 |
|
POM |
2-4 |
190-220 |
|
PA6 |
3-6 |
250-290 |
|
PA66 |
3-6 |
270-310 |
|
PP |
1-3 |
170-230 |
|
ABS |
2-3 |
180-260 |
|
PMMA |
3-4 |
210-250 |
|
PA/ABS |
2-4 |
230-270 |
|
PPO |
2-4 |
250-300 |